12,900+ practice questions · 144 exams · new questions added every week
Practice questions › Coating inspector › Coating & corrosion

Coating inspector Coating & corrosion practice questions

10 free questions with answers and explanations. Try each one, then tap “Show answer”.

  1. Corrosion

    1. Which form of corrosion produces deep, localised holes?

    • A. Chalking
    • B. Pitting
    • C. Uniform corrosion
    • D. Mud cracking
    Show answer

    Answer: B. Pitting

    Pitting can perforate a wall with little overall metal loss.

  2. Coatings

    2. Two-pack epoxies and polyurethanes cure by

    • A. oxidation only
    • B. chemical reaction between base and curing agent
    • C. sunlight only
    • D. solvent evaporation only
    Show answer

    Answer: B. chemical reaction between base and curing agent

    Mixing ratio and pot life must be respected.

  3. Calculations

    3. A coating has 70% volume solids. What wet film thickness gives a dry film of 200 µm (no thinner)?

    • A. 140 µm
    • B. 400 µm
    • C. 270 µm
    • D. 286 µm
    Show answer

    Answer: D. 286 µm

    WFT = DFT × 100 ÷ VS = 200 × 100 ÷ 70 = 286 µm.

  4. Surface prep

    4. Which test checks compressed air for oil and water before blasting?

    • A. Blotter test (ASTM D4285)
    • B. Pull-off test
    • C. Holiday test
    • D. Bresle test
    Show answer

    Answer: A. Blotter test (ASTM D4285)

    Contaminated air puts oil on the steel.

  5. Calculations

    5. A coating has 60% volume solids and is specified at 100 µm DFT. What is the theoretical spreading rate? (m²/L = VS% × 10 ÷ DFT µm)

    • A. 7 m²/L
    • B. 3 m²/L
    • C. 6 m²/L
    • D. 60 m²/L
    Show answer

    Answer: C. 6 m²/L

    60 × 10 ÷ 100 = 6 m²/L.

  6. Failures

    6. Osmotic blistering is mainly caused by

    • A. low humidity
    • B. soluble salts left under the coating
    • C. too thin a primer only
    • D. sunlight
    Show answer

    Answer: B. soluble salts left under the coating

    Water is drawn through the film towards the salts.

  7. Calculations

    7. A 60% volume solids paint is thinned by 5%. What WFT gives 125 µm DFT? (WFT = DFT × (100 + thinner%) ÷ VS)

    • A. 208 µm
    • B. 71 µm
    • C. 219 µm
    • D. 198 µm
    Show answer

    Answer: C. 219 µm

    125 × (100 + 5) ÷ 60 = 219 µm.

  8. Calculations

    8. The dew point is 20 °C and the steel surface is 24 °C. Can coating go ahead (using the 3 °C rule)?

    • A. Only if relative humidity is 100%
    • B. No — the steel is less than 3 °C above the dew point
    • C. Yes — the steel is at least 3 °C above the dew point
    • D. Dew point does not matter for coating
    Show answer

    Answer: C. Yes — the steel is at least 3 °C above the dew point

    The margin is 4 °C; at least 3 °C is required.

  9. Coatings

    9. A zinc-rich primer protects steel mainly by

    • A. sacrificial (galvanic) protection
    • B. inhibitive pigments only
    • C. adding heat
    • D. barrier action only
    Show answer

    Answer: A. sacrificial (galvanic) protection

    Barrier coatings block water and oxygen; inhibitive coatings slow corrosion chemically.

  10. Defects

    10. Mud cracking is usually caused by

    • A. using the wrong colour
    • B. applying it too thin
    • C. cold steel only
    • D. applying the coating too thick
    Show answer

    Answer: D. applying the coating too thick

    Common with zinc-rich primers.

Want more Coating inspector Coating & corrosion questions?

Get fresh questions every day, focused on your weak topics, plus timed mock tests. Free to start.

Practise free in the web app Practise on Telegram

About the Coating inspector on Mock Night · Original practice questions; not affiliated with the exam board.